Advanced Search

    column
    INFLUENCE OF ANNEALING ON PROPERTIES OF AZO THIN FILMS PREPARED BY SOL-GEL METHOD
    CHEN Wen-wen, LV Jun, WANG Jian-min, TANG Wen-ming, LIU Jun-wu, WU Yu-cheng, ZHENG Zhi-xiang
    2007, 43(2): 55-58.
    Abstract PDF
    THE INTERFACE MIGRATION IN Co-Zn DIFFUSION COUPLES
    YANG Ze-liang, SONG Yu-qiang, LI Shi-chun
    2007, 43(2): 59-61.
    Abstract PDF
    CARCK ANALYSIS OF 4130X STEEL IN FLATTENING TEST
    MA Zhi-qing
    2007, 43(2): 62-63.
    Abstract PDF
    THE EFFECT OF QUENCHED AND TEMPERED PROCESS ON MECHANICAL PROPERTY OF 25Cr2MoVA STEEL
    LOU Chun-ling
    2007, 43(2): 64-66.
    Abstract PDF
    CHARACTERISTICS OF WORK HARDENING OF 18-8 TYPE AUSTENITE STAINLESS
    NA Shun-sang, CHEN Bin-kai
    2007, 43(2): 67-69.
    Abstract PDF
    A NEW WAY TO IMPROVE THE MEASUREMENT SENSITIVITY OF LEAKING MAGNETISM METHOD FOR FATIGUE CRACK DETECTION ON THE POLE
    XIA Yong-fa, HE Xue-hong, LI Qin-wei
    2007, 43(2): 70-73.
    Abstract PDF
    REPEATABILITY AND REPRODUCIBILITY OF NANOINDENTATION TEST RESULT
    WANG Chun-liang, WANG Bin, SHA Fei, YANG Li, YAN Guo-qiang, MA Chong-xian, BA Fa-hai
    2007, 43(2): 74-77.
    Abstract PDF
    A NEW TECHNIQUE FOR X-RAY STRESS MEASUREMENT BASED ON USING IMAGE PLATE
    HONG Bo, JIANG Chuan-hai
    2007, 43(2): 78-80.
    Abstract PDF
    PREPARATION AND APPLICATION OF ORGANOSILOXANE MODIFIED ACRYLATE LATEX
    ZHANG Hui, GAO Yu, YAO Qiao-pin
    2007, 43(2): 81-83.
    Abstract PDF
    THE PRESENT CONDITION AND DEVELOPING DIRECTION OF DIE STEELS,HEAT TREATMENT PROCESSES AND STANDARDS IN CHINA
    ZHU Zong-Yuan, CUI Kun
    2007, 43(2): 84-88.
    Abstract PDF
    FRACTURE ANALYSIS OF THE REVOLUTION AXIS FOR THE LOCOMOTIVE MAIN GENERATOR
    DU Shi-hong, QIU Jie
    2007, 43(2): 89-90.
    Abstract PDF
    CRACK ANALYSIS OF DRIVEN GEAR
    LIU Li
    2007, 43(2): 91-93.
    Abstract PDF
    FAILURE ANALYSIS OF SEALING WASHER
    LI Chuan-rui, DING Li
    2007, 43(2): 94-96.
    Abstract PDF
    ANALYSIS ON WORKING CRACKING OF RAIL
    WU Xiong-xian
    2007, 43(2): 97-99.
    Abstract PDF
    FRACTURE ANALYSIS FOR FORGED LINKS OF 45 STEEL DURING THE SAND BLASTING PROCESS
    WU Ping
    2007, 43(2): 100-102.
    Abstract PDF
    INTRODUCTION TO STEEL-DETERMINATION OF CONTENT OF NONMETALLIC INCLUSIONS-MICROGRAPHIC METHOD USING STANDARDS DIAGRAMS GB/T 10561-2005 (Continued)
    ,
    2007, 43(2): 103-107.
    Abstract PDF