YAO Shu-ping, DONG Xia, LI Xiao-ling, ZONG Guo-qing, CHEN Yu-xuan. Forging Internal Crack Analysis of Large Thick-walled Tube[J]. PHYSICAL TESTING AND CHEMICAL ANALYSIS PART A:PHYSICAL TESTING, 2009, 45(2): 111-113.
Citation:
YAO Shu-ping, DONG Xia, LI Xiao-ling, ZONG Guo-qing, CHEN Yu-xuan. Forging Internal Crack Analysis of Large Thick-walled Tube[J]. PHYSICAL TESTING AND CHEMICAL ANALYSIS PART A:PHYSICAL TESTING, 2009, 45(2): 111-113.
YAO Shu-ping, DONG Xia, LI Xiao-ling, ZONG Guo-qing, CHEN Yu-xuan. Forging Internal Crack Analysis of Large Thick-walled Tube[J]. PHYSICAL TESTING AND CHEMICAL ANALYSIS PART A:PHYSICAL TESTING, 2009, 45(2): 111-113.
Citation:
YAO Shu-ping, DONG Xia, LI Xiao-ling, ZONG Guo-qing, CHEN Yu-xuan. Forging Internal Crack Analysis of Large Thick-walled Tube[J]. PHYSICAL TESTING AND CHEMICAL ANALYSIS PART A:PHYSICAL TESTING, 2009, 45(2): 111-113.
Forging Internal Crack Analysis of Large Thick-walled Tube
On the inner wall surface through the cracks of large thick-walled tube for chemical composition analysis,hardness,mechanical testing,metallography inspection and analysis. The results showed that,inside large tube radial cracks due to the lack of time and forging heating-anvil approach improper use caused by forging the split.