    FRACTURE ANALYSIS OF 45 QUALITY ROUND STEEL

    • 45 Quality roud steel fractured during forging. It was analyzed by means of metallographical examination, chemical composition analysis and inclusion testing, the results show that the fracture was mainly caused by no-metallic inclusion.