    Analysis on the Reasons Causing Blisters on Surface of 7A04 Aluminum Alloy Products

    • The formation mechanism and basic characteristics of blisters on surface of 7A04 aluminum alloy products caused by stratification, high temperature oxidation and overburning were analyzed by means of macro and micro examination.