    热压制备穿孔顶头用钼合金的力学性能表征

    Characterization of mechanical properties of molybdenum alloy for piercing plug prepared by hot pressing

    • 摘要: 采用添加TiH2、ZrH2的方式制备了TZC和TZM两种钼合金,研究了烧结和热压处理后合金的显微组织和力学性能。结果表明:烧结后热压可以有效提高合金的密度,降低合金中夹杂物和孔洞的占比,使合金的致密度达到97.3%。两种合金热压后的力学性能显著提升,但烧结和热压态合金的拉伸断口均呈脆性断裂特征。采用热压工艺制备的两种钼合金顶头的使用寿命均较烧结态顶头的使用寿命延长了80%以上。

       

      Abstract: TZC and TZM molybdenum alloys were prepared by adding TiH2 and ZrH2. The microstructure and mechanical properties of the alloys after sintering and hot pressing were studied. The results show that hot pressing after sintering could effectively improve the density of the alloy, reduce the proportion of inclusions and pores in the alloy, and make the density of the alloy reach 97.3%. The mechanical properties of the two alloys were significantly improved after hot pressing, but the tensile fracture of the sintered and hot-pressed alloys showed brittle fracture characteristics. The service life of two kinds of molybdenum alloy plugs prepared by hot pressing process was more than 80% longer than that of sintered plugs.

       

    /